TMT of wire rod production line

Unshaped Reasons of Wire Coil

The main reasons for the poor circle formation of wire out of the laying head are as follows. (1) Too much tension between mills (2) There is a deviation on water-cooled section alignment, nozzle conduit is worn to cause the unstable operation of the mill. (3) Roll ring of pinch roller is worn badly. Inappropriate clamping force of the…

Quality Control of HRC Surface

The entrapped slag is one of the main defects on the surface of ultra-low carbon steel hot-rolled coil, the overall macroscopic morphology of the defect is black color or black – white  strip, and there is obvious difference with the base sheet, intermittent distribution along the rolling direction, the length varies, often accompanied by warping…

Ladle Slag Adhesion

In operation, continuous casting ladle will appear slag adhesion or tumor phenomenon, resulting in a reduction in the effective volume. As the slag is very hard, it tends to intermingle with cold steel, which makes ladle unpacking very difficult and increases the number of ladle unpacker damages and repairs. With the…

Seven Testing Methods For steel materials

Seven common material testing methods in steel material labs, composition, spectra, mass spectra, energy spectra, morphology, physical structure, and thermogravimetry. 1.Composition analysis Composition analysis can be divided into two types according to the analysis object and requirements: micro sample analysis and trace component analysis. 2.Spectral analysis 1) Atomic Absorption Spectrometry…